Aluminum Pipe Supplier in Mumbai, India

PIPES & TUBES
Metals Fabrica supplies seamless extruded, drawn and structural aluminum alloy pipe and tube in 2xxx, 5xxx, 6xxx and 7xxx alloys to ASTM B241, B210, B221 and B429 in the temper your design calls for.
Steel pipes and tubes in bundles on racks in an industrial warehouse
OVERVIEW

Aluminum Pipe Overview

Aluminum pipe weighs roughly one third as much as steel pipe of the same size, conducts heat well and forms a natural oxide layer that protects it in air, fresh water and many marine atmospheres. It is specified where weight, corrosion behaviour or thermal performance matter more than the high-temperature strength of steel, for example in vehicle and aircraft structures, marine fabrication, cryogenic lines and architectural frames.

The alloy series decides how the pipe gains strength. Non-heat-treatable 5xxx alloys such as 5083 rely on magnesium in solid solution and cold work, so they keep good strength after welding and resist seawater. Heat-treatable 6xxx alloys such as 6061 and 6063 are solution treated and aged to T4 or T6, giving a balance of strength, weldability and finish. The 2xxx (copper) and 7xxx (zinc) alloys, 2014 and 7075, reach the highest strengths but are not normally fusion welded and need protection in corrosive service.

Seamless pipe and tube is hot extruded from a hollow or pierced billet over a mandrel, so it has no die-weld seams, and is covered by ASTM B241. Drawn seamless tube to ASTM B210 is cold drawn from extruded hollows for closer tolerances and higher strain-hardened tempers. Extruded tube to ASTM B221 and structural pipe to ASTM B429 serve general and load-bearing uses. The temper letter (O, H112, H32, T4, T6, T73) is part of the order and sets the mechanical properties. Metals Fabrica checks alloy, temper and product standard together on every aluminum enquiry, since the temper letter determines the properties on the certificate.

  • Weight: density about 2.7 g/cm³ against about 7.85 g/cm³ for carbon steel.
  • Low-temperature service: aluminum alloys do not show a ductile-to-brittle transition, which suits cryogenic piping.
  • Ordering: specify alloy, temper, standard, size and schedule or OD and wall.
  • Material data: see the aluminium materials page for the alloy families.
TYPES & VARIANTS

Types of Aluminum Pipe

ASTM B241 Seamless Extruded Pipe

Hot extruded over a mandrel with no weld seam, supplied in NPS sizes and schedules for pressure, hydraulic and structural lines in 5xxx, 6xxx, 2014 and 7075 alloys.

ASTM B210 Drawn Seamless Tube

Cold drawn from extruded hollows for tighter OD and wall tolerances, smoother surfaces and strain-hardened tempers such as H32 and H34 in 5xxx alloys.

ASTM B429 Extruded Structural Pipe

6061 and 6063 structural pipe and tube for frames, handrails, towers and supports, extruded through bridge or porthole dies and ordered by size and schedule.

ASTM B221 Extruded Tube

Extruded round, square and rectangular tube for general engineering, machine frames and fabrications where pressure-rated seamless pipe is not required.

Heat-Treated Temper Pipe (T4, T6, T73)

Solution heat-treated and aged pipe in 6061, 6063, 2014 and 7075. T73 overaging in 7075 trades some strength for much better stress-corrosion resistance.

Annealed and As-Fabricated Pipe (O, H112)

Soft O temper for bending, flaring and forming, and H112 as-extruded material in non-heat-treatable 5052, 5083 and 5086 for welded marine construction.

SPECIFICATIONS

Aluminum Pipe Specifications

SpecificationDetails
Pipe and tube standardsASTM B241 / B241M (seamless pipe and seamless extruded tube), ASTM B210 / B210M (drawn seamless tube), ASTM B221 / B221M (extruded bars, shapes and tube), ASTM B429 / B429M (extruded structural pipe and tube)
ASME standardASME SB241 (adopted from ASTM B241); allowable stresses per ASME Section II Part D for the listed alloys and tempers
Alloys2014, 5052, 5083, 5086, 6061, 6063, 7075
Dimension and tolerance standardsASME B36.10M schedules; ANSI H35.2 dimensional tolerances for aluminum mill products
Size range1/8" NB to 12" NB; tube 3 mm to 250 mm OD
Wall thicknessSCH 5 to SCH 80, and other walls to order
Manufacturing typeSeamless extruded, cold drawn seamless, extruded structural
TempersO, H111, H112 (5xxx); H32, H34 drawn (5052, 5086); T4, T5, T6 (6xxx); T4, T6 (2014); T6, T73 (7075)
EndsPlain end, bevelled end, threaded
LengthRandom and cut lengths
TestingTension test, dimensional and visual inspection; hydrostatic, eddy-current or ultrasonic test when specified; PMI on request
DocumentationEN 10204 3.1 mill test certificate; EN 10204 3.2 with third-party inspection when the order requires it

Not every alloy is available in every standard, temper or size. State the alloy, temper and standard together in your enquiry.

CHEMICAL COMPOSITION

Aluminum Pipe Chemical Composition

Weight %, maximum unless a range is shown, per the Aluminum Association registrations listed in ASTM B241 Table 1.
GradeUNSSiFeCuMnMgCrZnTiAl
2014A920140.50 – 1.20.73.9 – 5.00.40 – 1.20.20 – 0.80.100.250.15Remainder
5052A950520.250.400.100.102.2 – 2.80.15 – 0.350.10–Remainder
5083A950830.400.400.100.40 – 1.04.0 – 4.90.05 – 0.250.250.15Remainder
5086A950860.400.500.100.20 – 0.73.5 – 4.50.05 – 0.250.250.15Remainder
6061A960610.40 – 0.80.70.15 – 0.400.150.8 – 1.20.04 – 0.350.250.15Remainder
6063A960630.20 – 0.60.350.100.100.45 – 0.90.100.100.10Remainder
7075A970750.400.501.2 – 2.00.302.1 – 2.90.18 – 0.285.1 – 6.10.20Remainder

Other elements: 0.05 max each, 0.15 max total for all alloys shown. Each grade page lists the full requirements for that alloy.

MECHANICAL PROPERTIES

Aluminum Pipe Mechanical Properties

Room-temperature tensile requirements for extruded seamless pipe and tube per ASTM B241 / B241M, shown for one common temper of each alloy.
Alloy and TemperTensile StrengthYield Strength (0.2% Offset)Elongation in 50 mm or 4D, min
2014-T6 (wall up to 12.5 mm)415 MPa (60 ksi) min365 MPa (53 ksi) min7%
5052-O170 – 240 MPa (25 – 35 ksi)70 MPa (10 ksi) min14%
5083-O270 – 350 MPa (39 – 51 ksi)110 MPa (16 ksi) min14%
5086-O240 – 315 MPa (35 – 46 ksi)95 MPa (14 ksi) min14%
6061-T6260 MPa (38 ksi) min240 MPa (35 ksi) min8 – 10%
6063-T6205 MPa (30 ksi) min170 MPa (25 ksi) min8 – 10%
7075-T6 (wall up to 6.3 mm)540 MPa (78 ksi) min485 MPa (70 ksi) min7%

Requirements change with temper and wall thickness; the lower elongation applies to thinner walls. Each grade page lists all tempers. Confirm against the edition named in your purchase order.

EQUIVALENT GRADES

Aluminum Pipe Equivalent Grades

Nearest international designations for the aluminum alloys supplied as pipe and tube.
GradeUNSEN AWISOJISDIN / Werkstoff Nr.
2014A92014EN AW-2014 (AlCu4SiMg)AlCu4SiMgA2014AlCuSiMn / 3.1255
5052A95052EN AW-5052 (AlMg2.5)AlMg2.5A5052AlMg2.5 / 3.3523
5083A95083EN AW-5083 (AlMg4.5Mn0.7)AlMg4.5Mn0.7A5083AlMg4.5Mn / 3.3547
5086A95086EN AW-5086 (AlMg4)AlMg4A5086AlMg4Mn / 3.3545
6061A96061EN AW-6061 (AlMg1SiCu)AlMg1SiCuA6061AlMgSiCu / 3.3211
6063A96063EN AW-6063 (AlMg0.7Si)AlMg0.7SiA6063AlMgSi0.5 / 3.3206
7075A97075EN AW-7075 (AlZn5.5MgCu)AlZn5.5MgCuA7075AlZnMgCu1.5 / 3.4365

Equivalents are approximate. Composition limits and temper properties under EN 755 and JIS H4080 can differ from ASTM B241, so order to the standard named in your specification.

APPLICATIONS

Aluminum Pipe Applications

Marine and Shipbuilding

5083 and 5086 pipe for deck piping, rails, masts and superstructure fittings, chosen because magnesium alloys hold up in seawater spray and keep strength after welding.

Aerospace and Defence Structures

High-strength 2014 and 7075 tube for machined fittings, struts and hydraulic or structural members where strength-to-weight ratio is the main design driver.

Transport and Vehicle Frames

6061-T6 tube for truck bodies, trailers, rail interiors and bicycle or equipment frames that need weldable, moderately strong and lightweight sections.

Architecture and Handrails

6063 structural pipe to ASTM B429 for railings, balustrades, canopies and curtain-wall framing, where a clean extruded surface takes anodising well.

Cryogenic and Gas Lines

5083 and 6061 piping for liquefied gas and air-separation service, using the toughness aluminum alloys keep at very low temperatures.

Heat Transfer and HVAC

Drawn seamless tube in 5052 and 6061 for heat exchangers, solar collectors and fluid lines that benefit from aluminum's thermal conductivity.

WHY METALS FABRICA

Why Choose Metals Fabrica for Aluminum Pipe?

  • Alloy and temper checked together: we confirm that the alloy, temper and standard on your drawing are a valid combination before quoting.
  • Grade guidance: help choosing between weldable 5xxx and 6xxx alloys and high-strength 2014 or 7075 for your load, environment and joining method.
  • Standard and dimensions reviewed: B241, B210, B221 or B429, NPS or OD, schedule or wall, length and end finish checked against the specification.
  • Documentation support: EN 10204 3.1 certificates showing chemistry and tensile results, with third-party inspection coordinated when the order requires it.
  • Delivery coordination: quotations for Aluminum Pipe based on confirmed availability, with dispatch arranged from Mumbai.
FAQ

Aluminum Pipe FAQs

ASTM B241 covers seamless pipe and seamless extruded tube in the hot-extruded condition or heat-treated tempers. ASTM B210 covers seamless tube that is cold drawn after extrusion, which gives closer dimensional tolerances, a smoother surface and access to strain-hardened tempers such as H32 and H34.

5083 and 5086 are the usual choices. Their magnesium content gives good resistance to seawater and marine atmospheres, and as non-heat-treatable alloys they lose relatively little strength when welded. 6061 is also used above the waterline.

5052, 5083, 5086, 6061 and 6063 are routinely welded by MIG or TIG. Heat-treated 6xxx alloys lose part of their T6 strength in the heat-affected zone, which design codes allow for. 2014 and 7075 are not normally fusion welded and are joined mechanically.

O is fully annealed and softest. H112 is the as-extruded condition of a non-heat-treatable alloy with minimum properties guaranteed. T6 means solution heat-treated and artificially aged, the common high-strength condition for 6061, 2014 and 7075.

Aluminum pipe is ordered in NPS sizes with ASME B36.10M schedule wall thicknesses, commonly SCH 5, 10, 40 and 80. Tube is ordered by outside diameter and wall thickness, with tolerances per ANSI H35.2.

REQUEST A QUOTE

Request a Quote for Aluminum Pipe

Send the alloy, temper, standard, size, schedule or wall, length, quantity and inspection requirements. We review your Aluminum Pipe specification and reply with price and availability.