EN 10216-1/2/3/4 Seamless Steel Tube Supplier in Mumbai

EN STANDARDS PIPE
Metals Fabrica supplies seamless steel tubes for pressure purposes to EN 10216 Parts 1 to 4, covering room-temperature, elevated-temperature, fine-grain and low-temperature grades for boilers and vessels.
Steel pipes and tubes in bundles on racks in an industrial warehouse
OVERVIEW

EN 10216 Seamless Steel Tube Overview

EN 10216 is the European product standard for seamless steel tubes used in pressure equipment and pressure piping. It is published in five parts; Parts 1 to 4 cover carbon, carbon-manganese and ferritic alloy steels, and Part 5 covers stainless steels. Each part sets chemical composition, tensile properties, impact energy, heat treatment, test category and inspection documents, while outside diameter and wall thickness follow EN 10220.

Part 1 covers non-alloy steels with specified room-temperature properties, P195, P235 and P265, each in TR1 (no impact test or aluminium requirement) or TR2 (impact tested, aluminium killed). Part 2 covers steels with specified elevated-temperature properties, from carbon grades such as P235GH and P265GH to molybdenum and chromium-molybdenum grades such as 16Mo3, 13CrMo4-5, 10CrMo9-10 and X10CrMoVNb9-1. Part 3 covers normalised fine-grain steels such as P355N and P460N, and Part 4 covers steels with specified low-temperature toughness, from P265NL to 9% nickel X10Ni9.

Choose the part by design condition: Part 1 for ambient utility and process lines, Part 2 when the design uses elevated-temperature proof strength, Part 3 for higher strength at moderate temperature and Part 4 for sub-zero service. Test category TC1 or TC2 sets the extent of NDT and leak testing. For welded equivalents of Part 1 grades, see EN 10217-1 P235TR1 pipe. Metals Fabrica identifies which EN 10216 part your grade belongs to and confirms the test category and inspection document, 3.1 or 3.2, before quoting.

  • Parts: -1 room temperature, -2 elevated temperature, -3 fine grain, -4 low temperature
  • Dimensions: EN 10220, OD and wall thickness
  • Test categories: TC1 or TC2 (TC2 adds NDT)
  • Delivery condition: normalised or normalising formed; alloy grades normalised and tempered or quenched and tempered
TYPES & VARIANTS

Types of EN 10216 Seamless Steel Tube

EN 10216-1 P235TR1 / TR2 Tube

Non-alloy tube with room-temperature properties; TR2 adds aluminium-killed steel, impact testing and tighter limits for pressure equipment needing traceable toughness.

EN 10216-2 P235GH / P265GH Tube

Carbon steel boiler and pressure tube with specified 0.2% proof strength at elevated temperature, used for feedwater, steam and header lines.

EN 10216-2 16Mo3 and 13CrMo4-5 Tube

Molybdenum and chromium-molybdenum tubes for superheaters and steam piping where creep strength and oxidation resistance above carbon-steel limits are needed.

EN 10216-2 10CrMo9-10 and X10CrMoVNb9-1 Tube

2.25Cr-1Mo and 9Cr-1Mo-V grades for high-pressure, high-temperature power-plant lines, offering higher creep rupture strength than lower-alloy grades at the same wall thickness.

EN 10216-3 Fine-Grain Tube

Normalised fine-grain P275NL1, P355N and P460N grades offering higher yield strength with good weldability for vessels and hydraulic lines.

EN 10216-4 Low-Temperature Tube

P265NL, 12Ni14 and X10Ni9 grades with impact energy guaranteed at sub-zero temperatures for refrigeration, LPG and cryogenic duty.

SPECIFICATIONS

EN 10216 Seamless Steel Tube Specifications

SpecificationDetails
Product standardEN 10216-1, EN 10216-2, EN 10216-3, EN 10216-4 (seamless tubes for pressure purposes)
Related ASME / ASTMNearest: ASTM A106, A179, A192, A333, A335 (approximate, not interchangeable)
Dimension standardEN 10220
Size range10.2 mm to 914 mm OD
Wall thickness1.0 mm to 60 mm and to order
Manufacturing typeSeamless, hot finished or cold finished
Heat treatmentNormalised or normalising formed (non-alloy); normalised and tempered or quenched and tempered (alloy grades)
Test categoryTC1 or TC2 per part; TC2 includes NDT for longitudinal imperfections
EndsPlain end, bevelled end
LengthRandom and fixed lengths
TestingTensile, flattening or ring tests, impact (where specified), leak tightness, NDT, dimensional and visual inspection
DocumentationEN 10204 3.1 inspection certificate; EN 10204 3.2 on request

Name the part, grade, test category and any options in your enquiry. ERW and SAW tubes fall under EN 10217, not EN 10216.

CHEMICAL COMPOSITION

EN 10216 Seamless Steel Tube Chemical Composition

EN 10216-1 and EN 10216-2 (non-alloy and alloy)

GradePartCSiMnPSCrMoOther
P195TR1 / TR2-10.130.350.700.0250.020 / 0.0150.300.08Ni 0.30; Cu 0.30
P235TR1 / TR2-10.160.351.200.0250.020 / 0.0150.300.08Ni 0.30; Cu 0.30
P265TR1 / TR2-10.200.401.400.0250.020 / 0.0150.300.08Ni 0.30; Cu 0.30
P235GH-20.160.351.200.0250.0200.300.08Al 0.020 min; Ni 0.30; Cu 0.30
P265GH-20.200.401.400.0250.0200.300.08Al 0.020 min; Ni 0.30; Cu 0.30
16Mo3-20.12 – 0.200.350.40 – 0.900.0250.0200.300.25 – 0.35Ni 0.30; Cu 0.30
13CrMo4-5-20.10 – 0.170.350.40 – 0.700.0250.0200.70 – 1.150.40 – 0.60Ni 0.30; Cu 0.30
10CrMo9-10-20.08 – 0.140.500.30 – 0.700.0250.0202.00 – 2.500.90 – 1.10Ni 0.30; Cu 0.30
X10CrMoVNb9-1-20.08 – 0.120.20 – 0.500.30 – 0.600.0200.0108.00 – 9.500.85 – 1.05V 0.18 – 0.25; Nb 0.06 – 0.10; N 0.030 – 0.070; Ni 0.40

Weight %, maximum unless a range or minimum is shown. Where two S values are given, the first is TR1 and the second TR2.

EN 10216-3 and EN 10216-4 (fine grain and low temperature)

GradePartCSiMnPSNiOther
P355N-30.200.500.90 – 1.700.0250.0200.50Al 0.020 min; Nb, V, Ti limits apply
P265NL-40.200.400.60 – 1.400.0250.0200.30Al 0.020 min
12Ni14-40.150.350.30 – 0.800.0250.0103.25 – 3.75–
X10Ni9-40.100.350.30 – 0.800.0200.0108.50 – 10.00–

Weight %, maximum unless a range or minimum is shown. Values summarised for comparison; residual element limits are given in each part.

MECHANICAL PROPERTIES

EN 10216 Seamless Steel Tube Mechanical Properties

Minimum room-temperature properties for wall thickness T ≤ 16 mm, MPa (N/mm²). Yield strength reduces for thicker walls.
GradePartYield Strength ReH, minTensile Strength RmElongation A, min (long. / trans.)
P195TR1 / TR2-1195 MPa320 – 440 MPa27% / 25%
P235TR1 / TR2-1235 MPa360 – 500 MPa25% / 23%
P265TR1 / TR2-1265 MPa410 – 570 MPa21% / 19%
P235GH-2235 MPa360 – 500 MPa25% / 23%
P265GH-2265 MPa410 – 570 MPa23% / 21%
16Mo3-2280 MPa450 – 600 MPa22% / 20%
13CrMo4-5-2290 MPa440 – 590 MPa22% / 20%
10CrMo9-10-2280 MPa480 – 630 MPa22% / 20%
X10CrMoVNb9-1-2450 MPa630 – 830 MPa19% / 17%
P355N-3355 MPa490 – 650 MPa22% / 20%
P265NL-4265 MPa410 – 570 MPa24% / 22%

Impact energy requirements (TR2, Part 2, Part 3 and Part 4 grades) and elevated-temperature proof strength values are given in each part. Density of these steels is typically 7.85 g/cm³.

EQUIVALENT GRADES

EN 10216 Seamless Steel Tube Equivalent Grades

GradeMaterial No.ASTMJISBSGB
P235TR21.0255A106 Grade A (approx.)STPG 370BS 3601 36010
P235GH1.0345A106 Grade A / A192STPT 370BS 3602 HFS 360–
P265GH1.0425A106 Grade BSTPT 410BS 3602 HFS 41020G
16Mo31.5415A335 P1STPA 12–15MoG
13CrMo4-51.7335A335 P11 / P12STPA 22 / STPA 23BS 3604 620-44015CrMoG
10CrMo9-101.7380A335 P22STPA 24BS 3604 62212Cr2MoG
X10CrMoVNb9-11.4903A335 P91STPA 28–10Cr9Mo1VNbN
P265NL1.0453A333 Grade 6 (approx.)STPL 380BS 3603 430LT16MnDG (approx.)

Equivalents are approximate. Elevated-temperature strength, impact temperature and testing differ between systems; order to the standard required by your pressure code.

APPLICATIONS

EN 10216 Seamless Steel Tube Applications

Steam Boilers and Headers

P235GH, P265GH and 16Mo3 tubes for economisers, evaporators and headers designed with the elevated-temperature proof strength values of EN 10216-2.

Superheaters and Main Steam Lines

13CrMo4-5, 10CrMo9-10 and X10CrMoVNb9-1 tubes for high-temperature steam in power and process plants, where long-term creep rupture strength governs the required wall thickness.

Pressure Vessels and Heat Exchangers

Part 1 and Part 3 grades used for nozzles, shell tubes and exchanger bundles in process plants built to EN 13445.

Refrigeration and Gas Processing

EN 10216-4 P265NL and nickel steels with guaranteed impact energy at low temperatures for ammonia, LPG and ethylene service.

Hydraulic and Compressed-Air Lines

Fine-grain P355N and P460N tubes giving higher allowable stress, which allows thinner, lighter walls in high-pressure hydraulic and compressed-air systems.

Utility and Process Piping

P235TR1 and P235TR2 tube for water, air and process lines at ambient temperature, with TR2 chosen when impact testing is required.

WHY METALS FABRICA

Why Choose Metals Fabrica for EN 10216 Seamless Steel Tube?

  • Correct part and grade: we check that the grade, part number and quality (TR1, TR2, GH, N, NL) match your design temperature and pressure code.
  • Test category confirmed: TC1 or TC2, impact test temperature and any optional tests are reviewed before quoting.
  • Dimensions to EN 10220: OD and wall are checked against the standard series or your calculated minimum wall.
  • Complete pressure packages: tube quoted with alloy steel fittings and alloy steel flanges for Cr-Mo systems.
  • Documentation support: EN 10204 3.1 certificates, with 3.2 inspection coordinated when your notified body or client requires it.
FAQ

EN 10216 Seamless Steel Tube FAQs

EN 10216-1 tubes have specified room-temperature properties only. EN 10216-2 tubes also have specified 0.2% proof strength at elevated temperatures, and include molybdenum and chromium-molybdenum grades, so they are used where the design temperature is above ambient.

TR1 grades have no aluminium or impact energy requirements. TR2 grades are aluminium killed, have tighter limits on some elements and must meet impact energy requirements, which makes them suitable where pressure codes ask for proven toughness.

The test category sets the extent of inspection. TC2 adds non-destructive testing for longitudinal imperfections and other checks to the TC1 programme, and is usually required for more critical pressure equipment.

P265GH is usually compared with ASTM A106 Grade B, since both are carbon steel pressure grades with similar strength. The tensile and yield requirements and elevated-temperature data differ, so they are not automatically interchangeable.

EN 10216-4 covers non-alloy and alloy steel tubes with specified low-temperature properties, such as P265NL, 12Ni14 and X10Ni9. Each grade has a minimum impact energy at a defined sub-zero test temperature.

Outside diameters and wall thicknesses follow EN 10220, which lists preferred series for seamless and welded steel tubes. Tolerances on OD and wall are set in EN 10216 itself.

REQUEST A QUOTE

Request a Quote for EN 10216 Seamless Steel Tube

Send the EN 10216 part, grade, test category, OD and wall, length, quantity, impact or optional tests and the inspection document required. We review it and reply with price and availability.