ASTM A105 Bar Supplier in Mumbai, India

CARBON STEEL BARS
Metals Fabrica supplies ASTM A105 / ASME SA105 carbon steel bar, hot rolled or forged, for machining flanges, fittings and valve components, including normalised bar ordered as A105N.
Steel bars and rods
OVERVIEW

ASTM A105 Bar Overview

ASTM A105 is the standard for carbon steel forgings for piping applications: flanges, fittings, valves and similar parts for ambient and higher-temperature pressure systems. It is a forging standard, not a bar standard, but it allows hollow cylindrical parts of limited size to be machined from hot-rolled or forged bar when the axis of the part lies approximately parallel to the flow lines of the bar. A105 bar is therefore bar stock produced, heat treated where required and tested to meet the chemistry and properties of A105, so that parts machined from it can be certified to the same standard as forged ones.

Chemically, A105 is a carbon-manganese steel with carbon up to 0.35% and manganese 0.60–1.05%, plus residual limits on copper, nickel, chromium, molybdenum and vanadium. The minimum tensile strength is 485 MPa, minimum yield 250 MPa and hardness is capped at 187 HBW, which keeps the material machinable and weldable. Heat treatment by annealing, normalising or quench and temper is required for some part types and pressure classes; many buyers simply specify normalised material, often called A105N.

A105 has no impact test requirement. For low-temperature service, choose ASTM A350 LF2 bar instead. Metals Fabrica supplies A105 bar with the heat treatment and tests your purchase order states, and can quote matching ASTM A105 flanges and A105 forged fittings.

  • Standard: ASTM A105 / ASME SA105 (UNS K03504)
  • Strength: 485 MPa tensile, 250 MPa yield, minimum
  • Hardness: 187 HBW maximum
  • Bar use: machined hollow cylindrical parts within the size limit of the standard
TYPES & VARIANTS

Types of ASTM A105 Bar

A105 Hot-Rolled Round Bar

Black hot-rolled rounds certified to A105 for machining couplings, half couplings, plugs and small socket-weld or threaded fittings.

A105 Forged Round Bar

Forged rounds in larger diameters for machined flanges, hubs and valve components, with ultrasonic testing available for internal soundness.

A105N Normalised Bar

A105 bar normalised to refine grain size and give uniform properties, often specified by refineries and EPC contractors for all pressure parts.

A105 Hex Bar

Hexagon sections for hex-head plugs, bushings, unions and fittings, reducing machining time and material loss compared with turning the same parts from round stock.

A105 Peeled and Turned Bar

Bar with the decarburised surface removed and a controlled diameter, suited to CNC machining of valve stems, bonnets and fittings.

SPECIFICATIONS

ASTM A105 Bar Specifications

SpecificationDetails
StandardASTM A105 / ASME SA105 (forging standard; bar stock certified to it)
UNSK03504
ShapesRound, hexagon, square; forged rounds and blocks
Size range3 mm to 500 mm round; hex and square to order
Length1 to 6 m random, fixed and cut lengths
ConditionAs rolled or as forged where permitted; annealed, normalised (A105N), normalised and tempered, or quenched and tempered
FinishBlack, peeled, turned, bright
Toleranceh9, h11 or k12 for bright bar (typical)
TestingTensile and hardness per A105; ultrasonic testing, PMI and supplementary requirements on request
DocumentationEN 10204 3.1 mill test certificate; EN 10204 3.2 on request

State the part type and pressure class if heat treatment is required by the standard, and whether A105N is specified.

CHEMICAL COMPOSITION

ASTM A105 Bar Chemical Composition

Weight %, maximum unless a range is shown, per ASTM A105.
GradeUNSCMnSiPSCuNiCrMoV
A105K035040.350.60 – 1.050.10 – 0.350.0350.0400.400.400.300.120.08

Cu + Ni + Cr + Mo + V shall not exceed 1.00% and Cr + Mo shall not exceed 0.32%. For each 0.01% carbon below 0.35%, manganese may increase by 0.06% above 1.05%, up to 1.35%.

MECHANICAL PROPERTIES

ASTM A105 Bar Mechanical Properties

Minimum requirements per ASTM A105, with typical physical properties.
GradeDensityTensile Strength, minYield Strength, minElongation in 50 mm, minReduction of Area, minHardness, max
A1057.85 g/cm³485 MPa (70 ksi)250 MPa (36 ksi)22% (round specimen); 30% (strip)30%187 HBW

Density is a typical value, not a specification requirement.

EQUIVALENT GRADES

ASTM A105 Bar Equivalent Grades

GradeUNSEN / DINJISBSGBIS
ASTM A105K03504P250GH (1.0460)SFVC 2A–––

Equivalents are approximate. EN 10222-2 P250GH and JIS G3202 SFVC 2A differ in chemistry and testing; order to the standard in your specification.

APPLICATIONS

ASTM A105 Bar Applications

Socket-Weld and Threaded Fittings

Couplings, half couplings, caps, plugs and unions machined from A105 bar for ASME B16.11 small-bore piping in refineries and plants.

Small Flanges and Hubs

Machined flanges and hubs within the size limit the standard permits for bar stock, used in carbon steel process and utility lines.

Valve Bodies, Bonnets and Stems

Gate, globe and check valve components for ambient and high-temperature carbon steel systems in oil, gas and power service.

Instrumentation and Manifold Blocks

Bar machined into gauge connections, bleed rings, instrument manifolds and thermowell bodies that must carry the same A105 certification as the carbon steel piping.

Boiler and Steam Piping Parts

Nipples, bosses and connection pieces in steam and feedwater systems, where A105 is accepted for elevated-temperature pressure service.

WHY METALS FABRICA

Why Choose Metals Fabrica for ASTM A105 Bar?

  • Bar-stock acceptance checked: we confirm that the part you will machine is one A105 allows from bar, and flag where a forging is needed.
  • Heat treatment stated: normalised or Q&T condition confirmed on the certificate when your order or pressure class requires it.
  • Hardness controlled: 187 HBW maximum checked, with lower limits noted for sour-service orders.
  • Matched components: Metals Fabrica can supply A105 bar together with A105 flanges and forged fittings.
FAQ

ASTM A105 Bar FAQs

No. A105 covers carbon steel forgings for piping components. It allows certain hollow cylindrical parts to be machined from hot-rolled or forged bar, so bar is produced and certified to A105 chemistry and properties for that purpose.

A105N is not a separate grade. It means A105 material supplied in the normalised condition, which some purchasers require for all parts. The normalising requirement should be written into the order.

ASTM A105 limits hardness to 187 HBW. Sour-service specifications based on NACE MR0175 / ISO 15156 may set additional limits for carbon steel, which must be stated in the enquiry.

A105 has no Charpy impact requirement, so it is not intended for low-temperature service. ASTM A350 LF2 is the usual alternative where impact testing at −46 °C or −18 °C is required.

REQUEST A QUOTE

Request a Quote for ASTM A105 Bar

Send the shape, diameter, length, condition (as rolled, A105N or Q&T), quantity, the part to be machined and test requirements. Metals Fabrica will confirm price and availability.