ASTM A105 Forged Fittings Supplier in Mumbai, India

CARBON STEEL PIPE FITTINGS
Metals Fabrica supplies ASTM A105 / ASME SA105 carbon steel forged fittings in socket-weld and threaded Classes 2000 to 9000 to ASME B16.11, plus MSS SP-79, SP-83, SP-95 and SP-97 items.
Pipe fittings
OVERVIEW

ASTM A105 Forged Fittings Overview

ASTM A105 forged fittings are carbon steel socket-weld and threaded fittings machined from A105 forgings or forged bar, used for small-bore piping of NPS 4 and below. ASTM A105 is the material standard for carbon steel forgings for piping components at ambient and higher temperatures; ASME B16.11 sets their dimensions, tolerances and pressure classes. Together they cover elbows, tees, crosses, couplings, caps, plugs and bushings.

A105 steel has up to 0.35% carbon with 0.60–1.05% manganese, giving a minimum tensile strength of 485 MPa and yield of 250 MPa, with hardness limited to 187 HBW. Fittings may be supplied as forged or heat treated by annealing, normalising, or normalising and tempering; the standard makes heat treatment mandatory in specified cases, for example for higher-pressure flanges and fittings with welded ends in some services. Socket-weld fittings are rated Class 3000, 6000 or 9000 and threaded fittings Class 2000, 3000 or 6000.

A105 fittings are used with A106 Grade B pipe in the same lines as A234 WPB butt-weld fittings. A105 is not impact tested, so for low-temperature small-bore service A350 LF2 forgings are used instead. Metals Fabrica supplies A105 forged fittings in the class and end connection specified in your piping class.

  • Material: ASTM A105 / ASME SA105
  • Dimensions: ASME B16.11; MSS SP-79, SP-83, SP-95, SP-97
  • Strength: 485 MPa tensile, 250 MPa yield, 187 HBW max
  • Size range: 1/8″ to 4″ NB
TYPES & VARIANTS

Types of ASTM A105 Forged Fittings

A105 Socket-Weld Elbows and Tees

90° and 45° elbows, tees and crosses in Class 3000, 6000 and 9000, fillet welded to Schedule 80, 160 or XXS pipe in process lines.

A105 Threaded NPT Fittings

Class 2000, 3000 and 6000 threaded elbows, tees and crosses to ASME B16.11 for utility, instrument air and low-hazard small-bore lines.

A105 Couplings, Half Couplings and Caps

Full couplings for joining pipe, half couplings for vessel and pipe branch connections, and caps for closing socket-weld or threaded ends.

A105 Unions to MSS SP-83

Socket-weld and threaded unions in Class 3000 and 6000 that let pumps, valves and instruments be removed without cutting pipe.

A105 Swage Nipples, Plugs and Bushings

Swage nipples and bull plugs to MSS SP-95, hex head plugs and bushings for size reductions and closures in small-bore carbon steel piping.

A105 Branch Outlets (Olets)

Weldolets, sockolets, threadolets and nipolets to MSS SP-97 for reinforced branch connections from a larger run pipe, avoiding a full-size reducing tee in the header.

SPECIFICATIONS

ASTM A105 Forged Fittings Specifications

SpecificationDetails
Material standardASTM A105 / ASME SA105
UNSK03504
Dimension standardASME B16.11 (socket weld and threaded)
Related standardsMSS SP-79 (reducer inserts), SP-83 (unions), SP-95 (swage nipples, bull plugs), SP-97 (branch outlets)
Size range1/8" NB to 4" NB
Pressure classesSocket weld 3000, 6000, 9000; threaded 2000, 3000, 6000
ThreadsNPT to ASME B1.20.1; BSPT on request
Fitting typesElbows, tees, crosses, couplings, half couplings, caps, plugs, bushings, unions, swage nipples, olets
Heat treatmentAs forged, or annealed, normalised, or normalised and tempered where required by ASTM A105
FinishBlack, zinc plated, hot-dip galvanised or varnished as specified
TestingHardness (187 HBW max), tensile, dimensional and thread gauge checks, visual inspection; MPI on request
DocumentationEN 10204 3.1 mill test certificate; EN 10204 3.2 on request

Confirm the class, end connection, thread type and finish in your enquiry.

CHEMICAL COMPOSITION

ASTM A105 Forged Fittings Chemical Composition

Weight %, maximum unless a range is shown, per ASTM A105 Table 1.
GradeUNSCMnPSSiCuNiCrMoV
A105K035040.350.60 – 1.050.0350.0400.10 – 0.350.400.400.300.120.08

Cu + Ni + Cr + Mo + V must not exceed 1.00% and Cr + Mo must not exceed 0.32%. For each 0.01% carbon below 0.35%, Mn may increase by 0.06% up to 1.35%.

MECHANICAL PROPERTIES

ASTM A105 Forged Fittings Mechanical Properties

Room-temperature requirements per ASTM A105, with typical physical properties.
GradeDensityTensile Strength, minYield Strength, minElongation, minReduction of Area, minHardness, max
A1057.85 g/cm³485 MPa (70 ksi)250 MPa (36 ksi)22% (4D round); 30% (2 in strip)30%187 HBW

Density is a typical value, not a specification requirement. Confirm requirements against the purchase specification.

EQUIVALENT GRADES

ASTM A105 Forged Fittings Equivalent Grades

GradeUNSENDIN / W.Nr.JISMatching pipe grade
A105K03504P250GH (EN 10222-2)C22.8 / 1.0460SFVC 2AASTM A106 Gr B, A53 Gr B

Equivalents are approximate; strength levels differ between standards. Order to the standard named in your specification.

APPLICATIONS

ASTM A105 Forged Fittings Applications

Refinery and Petrochemical Small-Bore Piping

Socket-weld A105 fittings for drains, vents, sample and instrument connections on carbon steel process lines up to NPS 2.

Oil and Gas Wellhead and Production Facilities

Class 6000 and 9000 fittings for high-pressure chemical injection, sampling and instrument lines on production skids and manifolds.

Steam Tracing and Trap Assemblies

A105 tees, elbows and unions for steam trap stations and tracer lines, where forged fittings handle pressure and thermal cycling.

Compressed Air and Utility Networks

Threaded A105 fittings for plant air, nitrogen and water utility lines where field assembly without welding saves time.

Hydraulic and Lubrication Systems

High-class socket-weld and threaded fittings for hydraulic power units and lube oil skids that need compact, pressure-rated connections.

WHY METALS FABRICA

Why Choose Metals Fabrica for ASTM A105 Forged Fittings?

  • Class matched to schedule: we check that the B16.11 class corresponds to the pipe schedule in your line list.
  • End connection confirmed: socket weld, NPT or other threads, and the finish, are reviewed before quoting.
  • Matching components: A105 fittings quoted with ASTM A105 flanges and A106 Grade B pipe.
  • Documentation support: EN 10204 3.1 certificates showing hardness and heat treatment, with third-party inspection coordinated on request.
FAQ

ASTM A105 Forged Fittings FAQs

A105 covers forged fittings, which are machined into socket-weld and threaded fittings to ASME B16.11, normally NPS 4 and smaller. A234 WPB covers wrought butt-weld fittings to ASME B16.9 made from pipe or plate, used for larger lines.

ASTM A105 limits hardness to 187 HBW. Many sour-service specifications also require heat treatment and controlled hardness at welds, which should be stated in the order.

A105 is not impact tested, so its use at low temperature is restricted by the piping code. For impact-tested small-bore fittings, ASTM A350 LF2 forgings tested at −46 °C are normally specified.

For socket-weld fittings, Class 3000 corresponds to Schedule 80 pipe. For threaded fittings, Class 2000 corresponds to Schedule 80, with Class 3000 matched to Schedule 160.

REQUEST A QUOTE

Request a Quote for ASTM A105 Forged Fittings

List the fitting type, size, class, socket-weld or threaded ends, finish and quantity, with any heat treatment or inspection needs, and we will reply with a price.