Copper nickel 90/10 bar contains 9.0–11.0% nickel, 1.0–1.8% iron and up to 1.0% manganese in a copper matrix. The iron addition is essential: it helps form a tough, protective surface film in seawater that resists general corrosion, crevice attack and erosion at moderate flow speeds. ASTM B151 designates the alloy UNS C70600.
90/10 is the most widely used copper nickel for seawater systems because it balances corrosion resistance, good antifouling behaviour, weldability and cost. Compared with copper nickel 70/30 bar, it has lower strength and a lower tolerance for very high velocity or polluted water, but its resistance to biofouling is slightly better and it costs less. Bar parts in 90/10 are often specified to match 90/10 piping so the whole system is galvanically compatible.
Bar is extruded or hot rolled and supplied annealed or cold drawn to the tempers in B151, then peeled, turned or ground to size. It is not heat treatable; strength comes from cold work. Metals Fabrica supplies 90/10 bar with temper, finish and tolerance confirmed against your drawing, and can quote copper nickel 90/10 pipe for the same line.
Soft-annealed C70600 bar for parts that are formed, flared or extensively machined, giving the best ductility for seawater fittings.
Drawn temper with higher strength and a bright, close-tolerance surface for stems, pins and fasteners in seawater service.
Peeled or turned, then centreless ground bar for shafts and precision components that need straightness and a fine surface.
Hexagon stock for nuts, unions, plugs and adaptors in copper nickel seawater piping, cut to length or in random lengths.
Flat and rectangular sections for antifouling plates, marine brackets, earthing strips and other fabricated parts used in or near seawater.
| Specification | Details |
|---|---|
| Bar standard | ASTM B151 / ASME SB151 |
| UNS / grade | UNS C70600 (CuNi 90/10) |
| European standard | EN 12163 CW352H (CuNi10Fe1Mn) when named on the order |
| Shapes | Round, hex, square, flat, rectangular |
| Size range | 3 mm to 500 mm round; hex and square to order |
| Length | 1 to 6 m random, fixed and cut lengths |
| Temper | Annealed or cold-drawn tempers as listed in ASTM B151 |
| Finish | Black, bright, peeled, turned, centreless ground |
| Tolerance | Per ASTM B151; h9, h11 or k12 on request |
| Testing | Tensile, chemical analysis, PMI; hardness and ultrasonic testing on request |
| Documentation | EN 10204 3.1 mill test certificate; EN 10204 3.2 on request |
Confirm the temper, size and tolerance in your enquiry.
| Grade | UNS | Cu | Ni (incl. Co) | Fe | Mn | Pb | Zn |
|---|---|---|---|---|---|---|---|
| CuNi 90/10 | C70600 | Remainder | 9.0 – 11.0 | 1.0 – 1.8 | 1.0 | 0.05 | 1.0 |
Cu includes Ag.
| Grade and Temper | Density | Melting Range | Tensile Strength, min | Yield Strength, min |
|---|---|---|---|---|
| CuNi 90/10 (C70600), annealed | 8.94 g/cm³ | 1100 – 1145 °C | 260 MPa (38 ksi) | 105 MPa (15 ksi) |
Density and melting range are typical values, not specification requirements. Drawn tempers have higher, diameter-dependent minimums in ASTM B151.
| Grade | UNS | Werkstoff Nr. | EN / DIN | JIS | BS |
|---|---|---|---|---|---|
| CuNi 90/10 | C70600 | 2.0872 | CuNi10Fe1Mn (CW352H) | C7060 | CN102 |
Equivalents are approximate; iron and manganese ranges differ between standards. Order to the standard named in your specification.
Valve stems, strainer parts and fittings for engine cooling, ballast and firemain systems, matched to 90/10 piping for galvanic compatibility.
Machined parts for seawater lift, firewater deluge and utility water systems, where 90/10 offers reliable service at moderate velocity.
Bar and flat sections for intake screens, aquaculture fittings and sheathing hardware that use copper nickel's natural resistance to biofouling.
Tie rods, spacers and tube-sheet fasteners in seawater-cooled heat exchangers built with 90/10 tubes and tube sheets, keeping the bundle in one alloy.
Components in the cooler stages and seawater intake of desalination plants, where 90/10 gives good life at lower cost than 70/30.
The 1.0–1.8% iron helps the protective surface film form and greatly improves resistance to erosion-corrosion in flowing seawater. Without it, the alloy would corrode faster at moderate velocities.
90/10 copper nickel is UNS C70600. The nearest DIN / EN designations are 2.0872 and CW352H (CuNi10Fe1Mn).
Annealed C70600 bar is typically required to meet about 260 MPa (38 ksi) minimum tensile strength. Drawn tempers are stronger, and exact minimums depend on temper and diameter in ASTM B151.
Yes. It is readily welded by TIG or MIG, normally with 70/30 copper nickel filler metal, which gives a weld with corrosion resistance at least equal to the base metal.