ASTM A234 Gr WP22 Alloy Steel Pipe Fittings Supplier in Mumbai

ALLOY STEEL PIPE FITTINGS
Metals Fabrica supplies ASTM A234 / ASME SA234 WP22 2¼Cr-1Mo butt-weld fittings in Class 1 and Class 3 for A335 P22 steam and hydroprocessing lines, plus A182 F22 forgings.
Pipe fittings
OVERVIEW

ASTM A234 Gr WP22 Alloy Steel Pipe Fittings Overview

ASTM A234 WP22 fittings are made from 2¼% chromium, 1% molybdenum steel, the workhorse alloy for high-temperature steam and high-pressure hydrogen piping. They are used with ASTM A335 P22 pipe in main steam and hot reheat lines, boiler headers and hydrocracker reactor circuits.

The higher molybdenum content (0.87–1.13%) gives WP22 noticeably better creep-rupture strength than WP11 at temperatures above about 480 °C, which allows thinner walls for the same design conditions. Unlike WP11, WP22 limits silicon to 0.50% max. It is supplied in two classes with one chemistry: Class 1 at 415–585 MPa tensile and 205 MPa yield, and Class 3 at 520–690 MPa tensile and 310 MPa yield. Fittings are normalised and tempered, and hardness is limited to 217 HBW.

For supercritical boilers and the hottest steam lines, WP22 is increasingly replaced by WP91, which carries much higher allowable stresses. WP22 remains the usual choice for hydrogen service because its behaviour under API 941 is well documented. Metals Fabrica supplies WP22 fittings with the class, heat treatment and hardness confirmed against your line specification.

  • Standard: ASTM A234 / ASME SA234 WP22 Class 1, Class 3
  • Composition: 2¼Cr-1Mo, Cr 1.90–2.60%, Mo 0.87–1.13%
  • Heat treatment: normalised and tempered
  • Forged equivalent: ASTM A182 F22 Class 1, Class 3
TYPES & VARIANTS

Types of ASTM A234 Gr WP22 Alloy Steel Pipe Fittings

A234 WP22 Class 1 Fittings

The standard WP22 strength level, 415 to 585 MPa tensile and 205 MPa yield, matching A335 P22 pipe in most power and refinery specifications.

A234 WP22 Class 3 Fittings

Same 2¼Cr-1Mo chemistry heat treated to 520 to 690 MPa tensile and 310 MPa yield, for heavy-wall and high-pressure designs.

A234 WP22 Long-Radius Elbows

90° and 45° long-radius elbows to ASME B16.9 for main steam and hot reheat routing, often in heavy schedules or specified minimum wall.

A234 WP22 Tees and Reducing Tees

Extruded or hot-pressed tees for steam headers and reactor piping, with crotch reinforcement sized for the run pipe pressure.

A234 WP22 Reducers and Caps

Concentric and eccentric reducers and butt-weld caps for size transitions, header ends and dead legs in 2¼Cr-1Mo steam and process lines.

A182 F22 Forged Fittings

Socket-weld and threaded fittings and olets in Class 3000, 6000 and 9000 forged from A182 F22 for drains, vents and instrument tappings.

SPECIFICATIONS

ASTM A234 Gr WP22 Alloy Steel Pipe Fittings Specifications

SpecificationDetails
Standard / gradeASTM A234 / ASME SA234 WP22 Class 1, WP22 Class 3
Forged fittingsASTM A182 / ASME SA182 F22 Class 1, Class 3
Dimension standardsASME B16.9, ASME B16.11, MSS SP-97
Size range1/2" NB to 48" NB butt-weld; 1/8" to 4" forged
Wall thicknessSCH 10 to SCH 160, STD, XS, XXS, or minimum wall to match the pipe
ConstructionSeamless or welded (marked W); forged socket-weld and threaded
Heat treatmentNormalised and tempered, or annealed, per ASTM A234
Hardness217 HBW max
EndsBevelled to ASME B16.25; socket weld; NPT threaded
TestingTensile and hardness tests, dimensional and visual inspection, radiography of welds; UT, MPI and PMI on request
DocumentationEN 10204 3.1 certificate; EN 10204 3.2 on request

For hydrogen service, include any additional hardness, toughness or step-cooling requirements from your project specification.

CHEMICAL COMPOSITION

ASTM A234 Gr WP22 Alloy Steel Pipe Fittings Chemical Composition

Weight %, maximum unless a range is shown, per ASTM A234 Table 1.
GradeCMnPSSiCrMo
WP22 Class 1, Class 30.05 – 0.150.30 – 0.600.0400.0400.501.90 – 2.600.87 – 1.13
MECHANICAL PROPERTIES

ASTM A234 Gr WP22 Alloy Steel Pipe Fittings Mechanical Properties

Room-temperature tensile requirements per ASTM A234, with typical physical properties.
GradeTensile StrengthYield Strength, minElongation, min (longitudinal)Hardness, maxDensity
WP22 Class 1415 – 585 MPa (60 – 85 ksi)205 MPa (30 ksi)22%217 HBW7.83 g/cm³
WP22 Class 3520 – 690 MPa (75 – 100 ksi)310 MPa (45 ksi)22%217 HBW7.83 g/cm³

Density is a typical value, not a specification requirement. Elongation is for a standard round specimen in 4D.

EQUIVALENT GRADES

ASTM A234 Gr WP22 Alloy Steel Pipe Fittings Equivalent Grades

Fitting Grade (A234)Pipe (A335)Forging (A182)PlateEN (Material No.)JIS (pipe)GB (pipe)
WP22 Class 1P22F22 Class 1A387 Gr 22 Class 110CrMo9-10 (1.7380)STPA 2412Cr2MoG
WP22 Class 3P22F22 Class 3A387 Gr 22 Class 210CrMo9-10 (1.7380)STPA 2412Cr2MoG

Equivalents are close 2¼Cr-1Mo steels with differing strength requirements. Order to the standard in your specification.

APPLICATIONS

ASTM A234 Gr WP22 Alloy Steel Pipe Fittings Applications

Main Steam and Hot Reheat Lines

Elbows and tees in subcritical power plant steam piping, where 2¼Cr-1Mo creep strength supports long service at 540 °C and above.

Hydrocracker Reactor Piping

High-pressure hydrogen and hydrocarbon lines around hydrocracker reactors, where WP22 is selected for its documented resistance to high-temperature hydrogen attack.

Boiler Headers and Superheater Links

Header end caps, branch tees and link pipe fittings in superheater and reheater sections of utility and industrial boilers.

Refinery Heater Transfer Lines

Hot transfer piping from heaters to reactors and fractionators, where temperature and pressure exceed the economic range of WP11.

Combined-Cycle HRSG Piping

High-pressure superheater and steam outlet fittings in heat recovery steam generators, usually installed alongside WP91 components in the hottest sections.

WHY METALS FABRICA

Why Choose Metals Fabrica for ASTM A234 Gr WP22 Alloy Steel Pipe Fittings?

  • Class confirmed: we check whether your line class calls for WP22 Class 1 or Class 3 and quote the matching certificate.
  • Hydrogen service requirements captured: extra hardness, impact or step-cooling clauses are reviewed before quotation.
  • P22 piping packages: WP22 fittings, F22 forgings and A182 F22 flanges supplied together.
  • Documentation support: EN 10204 3.1 certificates with heat treatment records, and third-party inspection coordinated when needed.
FAQ

ASTM A234 Gr WP22 Alloy Steel Pipe Fittings FAQs

Both have the same 2¼Cr-1Mo chemistry. Class 1 requires 415–585 MPa tensile and 205 MPa yield; Class 3 requires 520–690 MPa tensile and 310 MPa yield, achieved by heat treatment.

ASTM A234 lists WP22 only in Class 1 and Class 3. The class numbers align the fitting strength levels with those of other A234 chrome-moly grades rather than forming a continuous series.

WP91 has much higher allowable stress at 550–600 °C, so it allows thinner walls in supercritical and high-temperature designs. WP22 remains common in subcritical plants and hydrogen service, and is easier to weld and heat treat.

WP22 fittings are used with ASTM A335 P22 pipe and ASTM A182 F22 flanges and forged fittings, in the class required by the piping specification.

ASTM A234 limits WP22 fittings to 217 HBW. Hydrogen and sour-service specifications often impose a lower limit, which should be stated in the enquiry.

REQUEST A QUOTE

Request a Quote for ASTM A234 Gr WP22 Alloy Steel Pipe Fittings

Send the class, fitting types, sizes, schedules or minimum walls, quantity and any hydrogen-service clauses, and we will reply with price and availability.