SS 446 Pipe Overview

SS 446 pipe is a ferritic stainless steel with 23–27% chromium, the highest chromium level of the common stainless grades, and very little nickel. The chromium gives excellent resistance to oxidation and scaling at high temperatures, and the low nickel content makes 446 more resistant than high-nickel austenitic grades to hot sulphur-bearing gases, where nickel sulphides can form. Up to 0.25% nitrogen helps limit grain growth during heating.

Pipe and tube are supplied to ASTM A268 in two variants. TP446-1 allows up to 0.20% carbon and has the higher minimum strength. TP446-2 limits carbon to 0.12%, which improves ductility and fabrication. Both are delivered annealed and are magnetic. As a ferritic grade, 446 has modest creep strength, a ductile-to-brittle transition close to room temperature in heavier sections, and can lose toughness after long exposure around 475 °C or in the sigma-forming range, so it is used mainly for non-pressure or low-stress hot parts.

Compared with SS 310 / 310S pipe, 446 is cheaper and better in sulphurous atmospheres, but weaker and less tough. For mechanical and wear service at lower temperatures, martensitic SS 410 pipe is the related choice. Flat products are listed under SS 446 sheets and plates. Metals Fabrica clarifies whether TP446-1 or TP446-2 is specified, since the two carry different carbon and property limits, and records that choice on the test certificate.

  • Standard: ASTM A268 / ASME SA268 TP446-1, TP446-2
  • Composition: 23–27% Cr, low nickel, up to 0.25% N
  • Strength: oxidation and sulphidation resistance at high temperature
  • Limitation: low creep strength and limited toughness
TYPES & VARIANTS

Types of SS 446 Pipe

A268 TP446-1 Seamless Tube

Higher-carbon variant with the higher minimum strength of the two, supplied annealed for furnace components and protection tubes.

A268 TP446-2 Tube

Carbon limited to 0.12% for better ductility, chosen when the tube will be bent, flared or welded into furnace and burner assemblies.

Thermocouple Protection Tubes

Closed-end or open-end 446 tubes that shield thermocouples and sensors in heat-treatment furnaces, salt baths and sulphur-bearing kiln atmospheres.

446 Radiant and Burner Tubes

Tubes for radiant heating elements, burner nozzles and flame tubes in furnaces, where scaling resistance matters more than load-bearing strength.

SPECIFICATIONS

SS 446 Pipe Specifications

SpecificationDetails
Product standardASTM A268 / ASME SA268 TP446-1, TP446-2 (seamless and welded tubing)
UNSS44600
Dimension standardsOD and wall per ASTM A268; NPS and schedule per ASME B36.19M / B36.10M where ordered as pipe
Size range1/8" NB to 24" NB seamless; up to 48" NB welded
Wall thicknessSCH 5S, 10S, 40S, 80S, 160, XXS
Manufacturing typeSeamless, welded
Delivery conditionAnnealed per ASTM A268
Ends and lengthPlain or bevelled; open or closed end for protection tubes; random or cut length
TestingHydrostatic or non-destructive electric test, flattening and flaring tests per A268; PMI on request
DocumentationEN 10204 3.1 mill test certificate; EN 10204 3.2 on request

State TP446-1 or TP446-2 on the order, as their carbon limits and strength differ.

CHEMICAL COMPOSITION

SS 446 Pipe Chemical Composition

Weight %, maximum unless a range is shown, per ASTM A268.
GradeUNSCMnSiPSCrNiN
TP446-1S446000.201.501.000.0400.03023.0 – 27.00.750.25
TP446-2S446000.121.501.000.0400.03023.0 – 27.00.500.25
MECHANICAL PROPERTIES

SS 446 Pipe Mechanical Properties

Minimum tensile requirements per ASTM A268 (annealed), with typical physical properties.
GradeTensile Strength, minYield Strength (0.2% Offset), minElongation in 50 mm, minDensityMelting Range
TP446-1485 MPa (70 ksi)275 MPa (40 ksi)18%7.50 g/cm³1425 – 1510 °C
TP446-2450 MPa (65 ksi)275 MPa (40 ksi)20%7.50 g/cm³1425 – 1510 °C

Density and melting range are typical values, not specification requirements. A268 also sets maximum hardness values; confirm them for your order.

EQUIVALENT GRADES

SS 446 Pipe Equivalent Grades

GradeUNSWerkstoff Nr.ENJISBSAFNORGOST
SS 446S446001.4749X18CrN28SUH 446––15Х28

Equivalents are approximate; 1.4749 has a narrower chromium range than S44600. Order to the standard named in your specification.

APPLICATIONS

SS 446 Pipe Applications

Furnace and Kiln Components

Radiant tubes, muffles, dampers and recuperator parts in furnaces and kilns, where 446 resists scaling in hot oxidising atmospheres.

Sulphur-Bearing Flue Gas

Hot gas ducts, soot blower parts and burner hardware in sulphur-rich combustion gases, where nickel-rich alloys can suffer sulphidation.

Thermocouple Sheaths

Protection tubes for temperature sensors in heat-treatment furnaces, glass tanks and non-ferrous melting, chosen for scaling resistance and low cost.

Glass and Ceramics Plants

Burner tubes, lehr components and kiln furniture supports where long exposure to hot air and combustion products requires high chromium.

WHY METALS FABRICA

Why Choose Metals Fabrica for SS 446 Pipe?

  • Variant confirmed: we check whether TP446-1 or TP446-2 suits your forming, welding and strength needs before quoting.
  • Service reviewed: temperature, atmosphere and loading are checked so that 446 is not used where creep strength or toughness is critical.
  • Dimensional basis agreed: OD and wall tube or NPS pipe sizes, end condition and lengths are confirmed against your drawing.
  • Documentation: EN 10204 3.1 certificates with chemistry and tensile results, and third-party inspection coordinated when required.
FAQ

SS 446 Pipe FAQs

TP446-1 allows up to 0.20% carbon and has higher minimum tensile strength. TP446-2 limits carbon to 0.12% for better ductility and formability, with a slightly lower tensile minimum.

446 resists oxidation in air to about 1100 °C, among the highest of the ferritic stainless steels. Its creep strength is low, so it is best for parts that carry little load at temperature.

446 contains little nickel, so it performs better than 310S in sulphur-bearing hot gases and costs less. 310S is stronger and tougher, so it is preferred for load-bearing or pressure parts.

446 has lower toughness than austenitic grades, especially in thick sections and at room temperature. Long exposure around 475 °C or in the sigma range can reduce toughness further, so handling and design should allow for this.

REQUEST A QUOTE

Request a Quote for SS 446 Pipe

Send the variant (TP446-1 or TP446-2), size, wall, end condition, operating temperature, atmosphere and quantity, and we will reply with price and availability.