ASTM A333 Grade 1 Pipe Supplier in Mumbai, India

CARBON STEEL PIPE
Metals Fabrica supplies ASTM A333 / ASME SA333 Grade 1 seamless and welded carbon steel pipe for low-temperature service, heat treated and Charpy impact tested at −45 °C (−50 °F).
Steel pipes and tubes in bundles on racks in an industrial warehouse
OVERVIEW

ASTM A333 Grade 1 Pipe Overview

ASTM A333 Grade 1 is a plain carbon-manganese pipe steel for low-temperature service. Like every A333 grade, it must pass a Charpy V-notch impact test at a set temperature, for Grade 1 −45 °C (−50 °F), which proves the pipe will not fail by brittle fracture when cold. ASME SA333 Grade 1 is the boiler-and-pressure-vessel code version.

Grade 1 has the lowest strength of the A333 carbon steel grades: 380 MPa (55 ksi) tensile and 205 MPa (30 ksi) yield minimum, with 35% longitudinal elongation. Its chemistry limits carbon to 0.30% and manganese to 0.40–1.06%, with phosphorus and sulphur held at 0.025% each, but, unlike A333 Grade 6, it has no silicon minimum. Toughness comes from heat treatment: the pipe is normalised, normalised and tempered, or, if seamless, finished from a controlled hot-working temperature.

Because Grade 6 offers the same −45 °C test with higher strength, most new projects specify Grade 6, and Grade 1 is chosen mainly where existing designs, thin-wall calculations or bending needs favour its lower strength and greater ductility. Pipe may be seamless or welded without filler metal. For colder duty, A333 Grade 3 is tested at −100 °C. Metals Fabrica checks that the A333 Grade 1 test certificate reports Charpy results at the temperature your piping class specifies, which may be colder than the standard value.

  • Standard: ASTM A333/A333M Grade 1, ASME SA333 Grade 1 (UNS K03008)
  • Impact test: Charpy V-notch at −45 °C (−50 °F)
  • Strength: 380 MPa tensile, 205 MPa yield minimum
  • Construction: seamless, or welded without filler metal
TYPES & VARIANTS

Types of ASTM A333 Grade 1 Pipe

A333 Grade 1 Seamless Pipe

Seamless pipe normalised or finished from a controlled hot-working temperature, then Charpy tested at −45 °C, for cold process lines that exclude weld seams.

A333 Grade 1 Welded Pipe

Electric-resistance-welded pipe made without filler metal, heat treated and impact tested, offering an economical low-temperature option in small and medium sizes.

Normalised and Tempered A333 Grade 1

Pipe normalised above 815 °C and then tempered, a route mills use to refine grain size and secure consistent impact energy through the wall.

Thin-Wall A333 Grade 1 Pipe

Light schedules where Grade 1's lower strength and higher elongation suit cold bending and forming, and where the design does not need Grade 6 strength.

SPECIFICATIONS

ASTM A333 Grade 1 Pipe Specifications

SpecificationDetails
StandardASTM A333/A333M Grade 1 / ASME SA333 Grade 1 (UNS K03008)
Dimension standardASME B36.10M
Size range1/8" NB to 36" NB seamless
Wall thicknessSCH 10 to SCH 160, STD, XS, XXS
Manufacturing typeSeamless; welded with no filler metal (ERW)
Heat treatmentNormalised at 815 °C (1500 °F) minimum, or normalised and tempered; seamless may be controlled hot finished
Impact testCharpy V-notch at −45 °C (−50 °F); full size 18 J average, 14 J single minimum
EndsPlain end, bevelled end (ASME B16.25)
LengthSingle random, double random, cut length
TestingTension, flattening, impact; hydrostatic or non-destructive electric test on each length
DocumentationEN 10204 3.1 certificate with impact results; EN 10204 3.2 on request

Very thin walls may be too thin for even the smallest Charpy specimen; A333 then waives or adjusts impact testing. Confirm size and wall in your enquiry.

CHEMICAL COMPOSITION

ASTM A333 Grade 1 Pipe Chemical Composition

Weight %, heat analysis, maximum unless a range is shown, per ASTM A333/A333M Table 1.
GradeUNSCMnPSSi
A333 Grade 1K030080.300.40 – 1.060.0250.025–

For each 0.01% reduction in carbon below 0.30%, manganese may increase by 0.05% above 1.06%, to a maximum of 1.35%.

MECHANICAL PROPERTIES

ASTM A333 Grade 1 Pipe Mechanical Properties

Minimum tensile and impact requirements per ASTM A333/A333M, with typical density.
GradeDensityTensile Strength, minYield Strength, minElongation in 50 mm, min (long. / trans.)Charpy Test TemperatureImpact Energy, min (10 × 10 mm)
A333 Grade 17.85 g/cm³380 MPa (55 ksi)205 MPa (30 ksi)35% / 25%−45 °C (−50 °F)18 J (13 ft·lbf) average of 3; 14 J (10 ft·lbf) single

Elongation is the basic minimum for strip and full-section specimens. Lower absorbed-energy values apply to sub-size Charpy specimens. Density is typical, not an A333 requirement.

EQUIVALENT GRADES

ASTM A333 Grade 1 Pipe Equivalent Grades

GradeUNSEN / DINJISBSGBIS
A333 Grade 1K03008P215NL (EN 10216-4) / TTSt 35 NSTPL 380 (JIS G3460)–––

Equivalents are approximate. Impact test temperature and energy differ between standards, so compare these values, not only the grade name.

APPLICATIONS

ASTM A333 Grade 1 Pipe Applications

Refrigeration and Chiller Plants

Brine, glycol and refrigerant lines in industrial cold stores and process chillers, where pipe must stay ductile at design temperatures well below zero.

Cold-Climate Utility Piping

Outdoor air, gas and water lines in regions where winter metal temperatures fall below the limits allowed for non-impact-tested carbon steel pipe.

Gas Let-Down and Depressurisation Lines

Piping downstream of pressure-reducing valves and blowdown lines, where gas expansion cools the pipe wall sharply during operation or emergency venting.

Replacement in Existing Grade 1 Systems

Maintenance and revamp work on plants originally designed with Grade 1, keeping the same material and strength basis as the original piping class.

WHY METALS FABRICA

Why Choose Metals Fabrica for ASTM A333 Grade 1 Pipe?

  • Grade 1 or Grade 6: we confirm whether your design requires Grade 1 or whether Grade 6, which is tested at the same temperature, is acceptable.
  • Impact data checked: test temperature, specimen size and absorbed energy are reviewed on the certificate before dispatch.
  • Low-temperature components: pipe quoted with ASTM A420 WPL6 fittings and ASTM A350 LF2 flanges.
  • Documentation support: EN 10204 3.1 certificates showing heat treatment and Charpy results, with third-party inspection coordinated when required.
FAQ

ASTM A333 Grade 1 Pipe FAQs

Both are Charpy tested at −45 °C. Grade 6 requires 0.10% minimum silicon and has higher strength, 415 MPa tensile and 240 MPa yield, against 380 MPa and 205 MPa for Grade 1. Grade 6 is the more common choice for new work.

With full-size 10 × 10 mm Charpy specimens, the average of three specimens must be at least 18 J (13 ft·lbf) and no single specimen below 14 J (10 ft·lbf). Proportionally lower values apply to sub-size specimens.

No. A333 permits seamless pipe and welded pipe made without filler metal, which in practice means electric-resistance welding. Large-diameter low-temperature welded pipe is normally ordered to ASTM A671.

Normalising refines the grain structure, which is what gives carbon steel its toughness at low temperature. The standard requires every A333 Grade 1 pipe to be treated to control its microstructure before impact testing.

REQUEST A QUOTE

Request a Quote for ASTM A333 Grade 1 Pipe

Send the size, schedule, length, seamless or welded, quantity, required impact energy if above the standard, and inspection needs. We will reply with price and availability.