ASTM A106 Grade C is the strongest of the three grades in the A106 seamless pipe standard. It shares the high-temperature purpose of Grade B but allows carbon up to 0.35%, which raises the minimum tensile strength to 485 MPa (70 ksi) and the minimum yield strength to 275 MPa (40 ksi). The higher allowable stress lets designers reduce wall thickness for the same pressure, saving weight on large, heavy-wall lines.
The manganese range (0.29–1.06%), the 0.035% limits on phosphorus and sulphur, the 0.10% silicon minimum and the residual limits are the same as for A106 Grade B; only carbon and strength differ. The extra carbon increases hardenability, so welding procedures for Grade C usually need closer control of preheat and heat input, and the carbon equivalent should be reviewed.
Grade C is produced in smaller volumes than Grade B, so lead time and minimum quantities should be checked early. Where the higher strength is not essential, Grade B is the practical choice; for large-diameter welded pipe of similar strength, see ASTM A672 C70 pipe. As Grade C is ordered less often than Grade B, Metals Fabrica confirms the grade, size and wall early in the enquiry and checks that the certificate reports Grade C tensile values.
Hot-rolled seamless pipe used as finished, with no further heat treatment required by the standard. This is the usual form for medium and large Grade C sizes.
Small-diameter Grade C pipe cold drawn for tighter tolerances and then heat treated at 650 °C or above after the last draw, as A106 requires.
Thick-wall pipe for high-pressure steam and process headers, where the higher allowable stress of Grade C reduces the wall needed compared with Grade B.
Pipe ordered with supplementary requirements such as product analysis, transverse tension or flattening tests, often specified for critical high-pressure service.
| Specification | Details |
|---|---|
| Standard | ASTM A106/A106M Grade C / ASME SA106 Grade C (UNS K03501) |
| Dimension standard | ASME B36.10M; A106 covers NPS 1/8 to NPS 48 |
| Size range | 1/8" NB to 36" NB seamless |
| Wall thickness | SCH 10 to SCH 160, STD, XS, XXS |
| Manufacturing type | Seamless: hot finished or cold drawn |
| Heat treatment | Hot-finished: none required; cold-drawn: 650 °C (1200 °F) minimum after final draw |
| Ends | Plain end, bevelled end (ASME B16.25) |
| Length | Single random, double random, cut length |
| Testing | Tension, bend test (NPS 2 and under), hydrostatic or non-destructive electric test; supplementary tests when ordered |
| Documentation | EN 10204 3.1 mill test certificate; EN 10204 3.2 on request |
Grade C is less widely produced than Grade B. Confirm size, wall, quantity and delivery time early in the enquiry.
| Grade | UNS | C | Mn | P | S | Si | Cr | Cu | Mo | Ni | V |
|---|---|---|---|---|---|---|---|---|---|---|---|
| A106 Grade C | K03501 | 0.35 | 0.29 – 1.06 | 0.035 | 0.035 | 0.10 min | 0.40 | 0.40 | 0.15 | 0.40 | 0.08 |
The five residual elements Cr, Cu, Mo, Ni and V together must not exceed 1.00%. Unless the purchaser specifies otherwise, manganese may exceed 1.06% by 0.06% for each 0.01% of carbon below 0.35%, up to 1.65%.
| Grade | Density | Melting Range | Tensile Strength, min | Yield Strength, min | Elongation in 50 mm, min (longitudinal / transverse) |
|---|---|---|---|---|---|
| A106 Grade C | 7.85 g/cm³ | ≈ 1415 – 1510 °C | 485 MPa (70 ksi) | 275 MPa (40 ksi) | 30% / 16.5% |
Elongation is the basic minimum for strip and full-section specimens; for standard round specimens the minimums are 20% longitudinal and 12% transverse. Density and melting range are typical, not A106 requirements.
| Grade | UNS | EN / DIN | JIS | BS | GB | IS |
|---|---|---|---|---|---|---|
| A106 Grade C | K03501 | – | STPT 480 (JIS G3456) | – | – | – |
Few standards have a direct counterpart to A106 Grade C; JIS STPT 480 is the closest match in strength. Equivalents are approximate; order to the standard named in your specification.
Large, heavy-wall steam and feedwater headers in power and process plants, where Grade C's higher allowable stress trims wall thickness, weight and support loads.
Hydrocarbon lines in hydroprocessing and reforming units that operate at elevated pressure and temperature but do not require chromium-molybdenum alloy pipe.
Boiler external piping under ASME Section I and B31.1, where SA106 Grade C provides strength without moving to alloy grades.
High-pressure hydraulic and pump discharge piping where designers want maximum carbon steel strength in a seamless pipe of manageable wall thickness.
Grade C has a higher allowable stress because its minimum tensile and yield strengths are 485 MPa and 275 MPa. On large, high-pressure lines this allows a thinner wall, reducing weight and welding time.
It can be. Grade C permits up to 0.35% carbon, so its carbon equivalent is usually higher. Welding procedures are typically qualified with controlled preheat and heat input, and hardness of the heat-affected zone may be checked.
A106 does not provide for dual certification between grades, and Grade C will not meet the 0.30% carbon maximum of Grade B if its carbon is above that level. Some heats may meet both; check the certificate if dual marking is needed.
ASTM A234 WPC wrought fittings and forgings of suitable strength are normally used with Grade C. Confirm the matching grades in your piping class, as many projects simply use WPB and A105 where the design allows.