ASTM A333 Grade 3 Pipe Supplier in Mumbai, India

CARBON STEEL PIPE
Metals Fabrica supplies ASTM A333 / ASME SA333 Grade 3 seamless and welded 3.5% nickel steel pipe, heat treated and Charpy impact tested at −100 °C (−150 °F) for cryogenic-range process lines.
Steel pipes and tubes in bundles on racks in an industrial warehouse
OVERVIEW

ASTM A333 Grade 3 Pipe Overview

ASTM A333 Grade 3 is a 3.5% nickel steel pipe for service far colder than plain carbon steel can tolerate. Where Grades 1 and 6 are impact tested at −45 °C, Grade 3 must pass a Charpy V-notch test at −100 °C (−150 °F). Strictly it is a low-alloy steel, but it is listed with the A333 carbon steel grades because it shares the same standard.

Nickel is the key element, held at 3.18–3.82%. It lowers the ductile-to-brittle transition temperature of the ferritic steel, so the pipe keeps its toughness in ethane, ethylene and propane service. Carbon is restricted to 0.19% maximum, manganese to 0.31–0.64% and silicon to 0.18–0.37%, with phosphorus and sulphur at 0.025% each. The resulting minimum strengths, 450 MPa (65 ksi) tensile and 240 MPa (35 ksi) yield, are higher than those of Grade 6.

Grade 3 pipe is normalised, or normalised and tempered, before impact testing, and welding requires nickel-bearing consumables and procedures qualified at the test temperature. For service down to −45 °C, Grade 1 or Grade 6 is more economical; for LNG temperatures near −196 °C, austenitic 304L stainless steel pipe or 9% nickel Grade 8 is used instead. On Grade 3 enquiries, Metals Fabrica confirms the nickel content, heat treatment and −100 °C impact results to be shown on the EN 10204 3.1 certificate.

  • Standard: ASTM A333/A333M Grade 3, ASME SA333 Grade 3 (UNS K31918)
  • Alloying: 3.18–3.82% nickel
  • Impact test: Charpy V-notch at −100 °C (−150 °F)
  • Strength: 450 MPa tensile, 240 MPa yield minimum
TYPES & VARIANTS

Types of ASTM A333 Grade 3 Pipe

A333 Grade 3 Seamless Pipe

Seamless 3.5% nickel steel pipe, the usual form for Grade 3, normalised and impact tested at −100 °C for ethylene and cold hydrocarbon process lines.

A333 Grade 3 Welded Pipe

Pipe welded without filler metal and heat treated after welding, with the weld and heat-affected zone included in the −100 °C impact test programme.

Normalised and Tempered Grade 3 Pipe

Normalised, then tempered to relieve stresses and stabilise toughness, a common route for heavier walls in the nickel steel grades.

Grade 3 Pipe with Enhanced Impact Requirements

Pipe ordered with higher absorbed-energy or lateral-expansion values than A333 minimums, as some ethylene and LNG project specifications require.

SPECIFICATIONS

ASTM A333 Grade 3 Pipe Specifications

SpecificationDetails
StandardASTM A333/A333M Grade 3 / ASME SA333 Grade 3 (UNS K31918)
Dimension standardASME B36.10M
Size range1/8" NB to 36" NB seamless
Wall thicknessSCH 10 to SCH 160, STD, XS, XXS
Manufacturing typeSeamless; welded with no filler metal
Heat treatmentNormalised, or normalised and tempered, to control microstructure
Impact testCharpy V-notch at −100 °C (−150 °F); full size 18 J average, 14 J single minimum
EndsPlain end, bevelled end (ASME B16.25)
LengthSingle random, double random, cut length
TestingTension, flattening, impact; hydrostatic or non-destructive electric test; PMI for nickel on request
DocumentationEN 10204 3.1 certificate with nickel content and impact results; EN 10204 3.2 on request

Grade 3 is a specialised grade with limited mill production. Confirm size, wall, quantity and delivery requirements early.

CHEMICAL COMPOSITION

ASTM A333 Grade 3 Pipe Chemical Composition

Weight %, heat analysis, maximum unless a range is shown, per ASTM A333/A333M Table 1.
GradeUNSCMnPSSiNi
A333 Grade 3K319180.190.31 – 0.640.0250.0250.18 – 0.373.18 – 3.82
MECHANICAL PROPERTIES

ASTM A333 Grade 3 Pipe Mechanical Properties

Minimum tensile and impact requirements per ASTM A333/A333M, with typical density.
GradeDensityTensile Strength, minYield Strength, minElongation in 50 mm, min (long. / trans.)Charpy Test TemperatureImpact Energy, min (10 × 10 mm)
A333 Grade 37.86 g/cm³450 MPa (65 ksi)240 MPa (35 ksi)30% / 20%−100 °C (−150 °F)18 J (13 ft·lbf) average of 3; 14 J (10 ft·lbf) single

Elongation is the basic minimum for strip and full-section specimens. Sub-size Charpy specimens have proportionally lower energy requirements. Density is a typical value for 3.5% nickel steel.

EQUIVALENT GRADES

ASTM A333 Grade 3 Pipe Equivalent Grades

GradeUNSEN / DINJISBSGBIS
A333 Grade 3K3191812Ni14 (EN 10216-4) / 1.5637STPL 450 (JIS G3460)BS 3603 503 LT100––

Equivalents are approximate; EN 10216-4 and JIS G3460 set their own impact temperatures and energies. Order to the standard named in your specification.

APPLICATIONS

ASTM A333 Grade 3 Pipe Applications

Ethylene and Olefin Plants

Cold-section piping around demethanisers, deethanisers and ethylene refrigeration circuits, where metal temperatures can fall close to −100 °C and carbon steel grades lack toughness.

LPG and Propane Refrigeration

Propane and propylene refrigerant loops and cold LPG storage connections, where nickel steel gives a safety margin below the −45 °C limit of Grade 6.

Gas Processing and NGL Recovery

Turbo-expander outlets, cold boxes and NGL fractionation lines in gas plants, where the gas is chilled to recover ethane and heavier liquids.

Air Separation and Industrial Gases

Warm-end and intermediate-temperature piping in air separation units and CO2 liquefaction plants that do not reach full cryogenic temperatures.

WHY METALS FABRICA

Why Choose Metals Fabrica for ASTM A333 Grade 3 Pipe?

  • Temperature-based grade check: we confirm your design temperature truly needs Grade 3 rather than Grade 6, or austenitic stainless for colder duty.
  • Nickel content verified: heat analysis on the certificate, with PMI coordinated on request to confirm the 3.5% nickel alloy.
  • Matching low-temperature parts: Grade 3 pipe can be quoted with A420 WPL3 fittings and A350 LF3 flanges when your piping class calls for them.
  • Impact results reviewed: −100 °C Charpy results and specimen size checked before dispatch, with third-party inspection coordinated when required.
FAQ

ASTM A333 Grade 3 Pipe FAQs

A333 Grade 3 is impact tested at −100 °C (−150 °F), which is the basis for its use down to about that temperature. The allowed minimum design metal temperature is set by the applicable piping code.

About 3.5% nickel lowers the ductile-to-brittle transition temperature of ferritic steel. This keeps the pipe tough at temperatures where plain carbon-manganese steel would become brittle.

No. LNG is stored and handled at about −162 °C, below the −100 °C test temperature of Grade 3. LNG piping normally uses austenitic stainless steel or 9% nickel steel such as A333 Grade 8.

The usual companions are ASTM A420 Grade WPL3 wrought fittings and ASTM A350 Grade LF3 forgings, which have the same 3.5% nickel basis and −100 °C impact test.

Yes. Welding normally uses nickel-bearing filler metal, and procedures must be qualified with impact tests on weld metal and heat-affected zone at the design temperature.

REQUEST A QUOTE

Request a Quote for ASTM A333 Grade 3 Pipe

Send the size, schedule, length, quantity, design temperature, any additional impact requirements and inspection needs, and we will reply with price and lead time.